上海口腔医学 ›› 2014, Vol. 23 ›› Issue (6): 689-694.

• 基础研究 • 上一篇    下一篇

不同表面处理方法对纤维桩与树脂黏结强度的影响

郑虎1, 郭建青1, 张献芳2   

  1. 1.上海市徐汇区大华医院 口腔科,上海 200237; 2.上海市徐汇区牙病防治所 口腔修复科,上海 200032
  • 收稿日期:2014-05-30 修回日期:2014-07-04 出版日期:2014-12-20 发布日期:2015-01-08
  • 通讯作者: 郭建青,E-mail:guojianqing111@163.com E-mail:dhyyzh@126.com
  • 作者简介:郑虎(1977-),男,硕士,主治医师
  • 基金资助:
    徐汇区科学技术委员会资助项目(SHXH201138)

Effect of different surface treatments on the bond strength of fiber posts to resin cement

ZHENG Hu, GUO Jian-qing, ZHANG Xian-fang   

  1. 1.Department of Stomatology, Dahua Hospital, Xuhui District. Shanghai 200237;
    2. Department of Prosthodontics, Dental Center of Xuhui District. Shanghai 200032, China
  • Received:2014-05-30 Revised:2014-07-04 Online:2014-12-20 Published:2015-01-08
  • Supported by:
    Research Project of Science and Technology Commission of Xuhui District (SHXH201138)

摘要: 目的: 比较5种不同表面处理方法对纤维桩黏结强度的影响。方法:50根纤维桩按照表面处理方法的不同,随机分为5组,A组为硅烷偶联剂组(Clearfil Porcelain Bond Activator,Kuraray),B组为硅烷偶联剂+黏结剂组(A+ Clearfil SE Bond,Kuraray),C组为过氧化氢组(30%H2O2溶液),D组为过氧化氢+硅烷偶联剂组(C+A),E组为对照组。分别与树脂黏结剂黏结后,每组再平均分成2个小组,1组37℃生理盐水保存24 h后进行微拉伸强度测试,1组37℃生理盐水保存24 h后进行10000次冷热循环再进行微拉伸强度测试。采用SPSS17.0软件包对数据进行统计学分析。结果:冷热循环前A组~E组的微拉伸黏结强度分别为(6.7±0.7)、(14.4±1.1)、(10.7±0.9)、(16.0±1.0)和(6.7±1.0) MPa,冷热循环后,A组~E组的微拉伸黏结强度分别为(6.0±0.7 )、(13.1±0.7)、(9.0±0.7)、(15.0±0.9 ) 和(5.6±0.7) MPa。除硅烷偶联剂组与对照组之间外,其余各组之间差异均有显著性(P<0.05),其中,过氧化氢+硅烷偶联剂组黏结强度最大。各组之间在冷热循环前、后的微拉伸黏结强度差异均有显著性(P<0.05)。结论:温度疲劳循环可以降低5种表面处理的纤维桩与树脂间的黏结强度,30%H2O2溶液处理纤维桩后再使用硅烷偶联剂,可显著增加纤维桩与树脂之间的黏结强度。

关键词: 纤维桩, 表面处理, 微拉伸测试, 冷热循环

Abstract: PURPOSE: To evaluate the effects of five different surface treatments on the bond strength between fiber posts and resin cement. METHODS: Fifty fiber posts were randomly divided into 5 groups for different surface treatments. Group A was treated with silane coupling agent (Clearfil Porcelain Bond Activator,Kuraray); Group B was treated with silane coupling agent and then coated with dentin bonding agent (Clearfil SE Bond,Kuraray); Group C was immersed in 30%H2O2; Group D was immersed in 30%H2O2 and then treated with silane coupling agent; Group E received no surface treatment (control group). After bonding to resin cement, each group was then divided into 2 subgroups equally,while one group was stored in sodium chloride for 24 h at 37℃, and the other group was stored in sodium chloride for 24 h at 37℃ and then subjected to thermal cycling for 10000 times. Microtensile bond strengths were tested and the data was statistically analyzed using SPSS17.0 software package. RESULTS: The microtensile bond strength before thermal cycling was(6.7±0.7) MPa for group A,(14.4±1.1) MPa for group B,(10.7±0.9) MPa for group C,(16.0±1.0) MPa for group D and (6.7±1.0) MPa for group E. After thermal cycling, the microtensile bond strength was (6.7±0.7) MPa for group A, (13.1±0.7) MPa for group B, (9.0±0.7) MPa for group C, (15.0±0.9) MPa for group D and (5.6±0.7) MPa for group E. The results showed that surface treatments had significant impact on the bond strength (P<0.05). There was no significant difference between group A and group E. Group D had the highest bond strength compared with the other groups. Microtensile bond strengths were significantly different before and after thermalcycling treatment in each group (P<0.05). CONCLUSIONS: Thermocycling treatment decreases the bond strength of fiber posts to resin cement with these 5 surface treatments. Coupled with 30%H2O2 solution and silanization, the bonding strength of fiber posts to resin cement can increase significantly.

Key words: Fiber posts, Surface treatment, Microtensil test, Thermocycling